Tracie 04-10-2007 01:32 PM

SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
I am going to be replacing the windshield hinges, upper and lower door
hinges, and hood hinges on my 2006 Wrangler X (just to prevent rust in
the future). I am torn between getting the 304 stainless steel with
the high polished mirror finish or the black chrome finish over the
304 stainless steel. My jeep is the Midnight Blue metallic (navy
blue) color. Which one would look better? I also am going to be
putting on nerf bars (preferably stainless) and would also like to
install the euro guard headlight/side marker/parking/tail light guards
but I am not sure which color of these yet (depends on the color of
all the hinges). Anyone have any suggestions or know anything about
the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
would be greatly appreciated. THANKS


Earle Horton 04-10-2007 02:03 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
I did that on my 1995 Wrangler when it was new. OK, the stainless doesn't
rust but that isn't why we do this sort of thing, now is it? The door and
windshield hinges are a sob to get adjusted right, and if you get the cheap
ones (any brand but Kentrol) you are going to be sorry. If you put Steel
Horse parts of any description on your Jeep you are going to be real sorry.
Stainless scratches if you touch it and then you make it look worse when you
try to polish it. The bolts that these parts tend to come with are a joke.
Go to your local Ace Hardware store and get some hex head cap screws in
stainless. You will love them. Much better than the Allen head joke screws
you get with stainless parts.

There is no such thing as "black chrome". The black hinges and such are
powder coated. This stuff chips and comes off unless it is primed right at
the factory, and sometimes even then.

Good luck.

Earle

"Tracie" <brainart@upstate.edu> wrote in message
news:1176226322.897231.185570@p77g2000hsh.googlegr oups.com...
> I am going to be replacing the windshield hinges, upper and lower door
> hinges, and hood hinges on my 2006 Wrangler X (just to prevent rust in
> the future). I am torn between getting the 304 stainless steel with
> the high polished mirror finish or the black chrome finish over the
> 304 stainless steel. My jeep is the Midnight Blue metallic (navy
> blue) color. Which one would look better? I also am going to be
> putting on nerf bars (preferably stainless) and would also like to
> install the euro guard headlight/side marker/parking/tail light guards
> but I am not sure which color of these yet (depends on the color of
> all the hinges). Anyone have any suggestions or know anything about
> the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
> would be greatly appreciated. THANKS
>




Earle Horton 04-10-2007 02:03 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
I did that on my 1995 Wrangler when it was new. OK, the stainless doesn't
rust but that isn't why we do this sort of thing, now is it? The door and
windshield hinges are a sob to get adjusted right, and if you get the cheap
ones (any brand but Kentrol) you are going to be sorry. If you put Steel
Horse parts of any description on your Jeep you are going to be real sorry.
Stainless scratches if you touch it and then you make it look worse when you
try to polish it. The bolts that these parts tend to come with are a joke.
Go to your local Ace Hardware store and get some hex head cap screws in
stainless. You will love them. Much better than the Allen head joke screws
you get with stainless parts.

There is no such thing as "black chrome". The black hinges and such are
powder coated. This stuff chips and comes off unless it is primed right at
the factory, and sometimes even then.

Good luck.

Earle

"Tracie" <brainart@upstate.edu> wrote in message
news:1176226322.897231.185570@p77g2000hsh.googlegr oups.com...
> I am going to be replacing the windshield hinges, upper and lower door
> hinges, and hood hinges on my 2006 Wrangler X (just to prevent rust in
> the future). I am torn between getting the 304 stainless steel with
> the high polished mirror finish or the black chrome finish over the
> 304 stainless steel. My jeep is the Midnight Blue metallic (navy
> blue) color. Which one would look better? I also am going to be
> putting on nerf bars (preferably stainless) and would also like to
> install the euro guard headlight/side marker/parking/tail light guards
> but I am not sure which color of these yet (depends on the color of
> all the hinges). Anyone have any suggestions or know anything about
> the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
> would be greatly appreciated. THANKS
>




Earle Horton 04-10-2007 02:03 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
I did that on my 1995 Wrangler when it was new. OK, the stainless doesn't
rust but that isn't why we do this sort of thing, now is it? The door and
windshield hinges are a sob to get adjusted right, and if you get the cheap
ones (any brand but Kentrol) you are going to be sorry. If you put Steel
Horse parts of any description on your Jeep you are going to be real sorry.
Stainless scratches if you touch it and then you make it look worse when you
try to polish it. The bolts that these parts tend to come with are a joke.
Go to your local Ace Hardware store and get some hex head cap screws in
stainless. You will love them. Much better than the Allen head joke screws
you get with stainless parts.

There is no such thing as "black chrome". The black hinges and such are
powder coated. This stuff chips and comes off unless it is primed right at
the factory, and sometimes even then.

Good luck.

Earle

"Tracie" <brainart@upstate.edu> wrote in message
news:1176226322.897231.185570@p77g2000hsh.googlegr oups.com...
> I am going to be replacing the windshield hinges, upper and lower door
> hinges, and hood hinges on my 2006 Wrangler X (just to prevent rust in
> the future). I am torn between getting the 304 stainless steel with
> the high polished mirror finish or the black chrome finish over the
> 304 stainless steel. My jeep is the Midnight Blue metallic (navy
> blue) color. Which one would look better? I also am going to be
> putting on nerf bars (preferably stainless) and would also like to
> install the euro guard headlight/side marker/parking/tail light guards
> but I am not sure which color of these yet (depends on the color of
> all the hinges). Anyone have any suggestions or know anything about
> the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
> would be greatly appreciated. THANKS
>




SnoMan 04-10-2007 02:40 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
<apodo@gracioso.usa> wrote:

>Stainless scratches if you touch it and then you make it look worse when you
>try to polish it.



It takes more than a touch to scratch it as it is pretty tuff and it
is not hard to polish out scratches if you do it right. You just need
the right method and compound.
-----------------
TheSnoMan.com

SnoMan 04-10-2007 02:40 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
<apodo@gracioso.usa> wrote:

>Stainless scratches if you touch it and then you make it look worse when you
>try to polish it.



It takes more than a touch to scratch it as it is pretty tuff and it
is not hard to polish out scratches if you do it right. You just need
the right method and compound.
-----------------
TheSnoMan.com

SnoMan 04-10-2007 02:40 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
<apodo@gracioso.usa> wrote:

>Stainless scratches if you touch it and then you make it look worse when you
>try to polish it.



It takes more than a touch to scratch it as it is pretty tuff and it
is not hard to polish out scratches if you do it right. You just need
the right method and compound.
-----------------
TheSnoMan.com

Tracie 04-10-2007 02:58 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>
> <a...@gracioso.usa> wrote:
> >Stainless scratches if you touch it and then you make it look worse when you
> >try to polish it.

>
> It takes more than a touch to scratch it as it is pretty tuff and it
> is not hard to polish out scratches if you do it right. You just need
> the right method and compound.
> -----------------
> TheSnoMan.com


I have heard of Kentrol. They are supposed to be good. Anybody know
anything about Rugged Ridge stainless hinges?


Tracie 04-10-2007 02:58 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>
> <a...@gracioso.usa> wrote:
> >Stainless scratches if you touch it and then you make it look worse when you
> >try to polish it.

>
> It takes more than a touch to scratch it as it is pretty tuff and it
> is not hard to polish out scratches if you do it right. You just need
> the right method and compound.
> -----------------
> TheSnoMan.com


I have heard of Kentrol. They are supposed to be good. Anybody know
anything about Rugged Ridge stainless hinges?


Tracie 04-10-2007 02:58 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>
> <a...@gracioso.usa> wrote:
> >Stainless scratches if you touch it and then you make it look worse when you
> >try to polish it.

>
> It takes more than a touch to scratch it as it is pretty tuff and it
> is not hard to polish out scratches if you do it right. You just need
> the right method and compound.
> -----------------
> TheSnoMan.com


I have heard of Kentrol. They are supposed to be good. Anybody know
anything about Rugged Ridge stainless hinges?


Mike Romain 04-10-2007 03:54 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
Tracie wrote:
> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>>
>> <a...@gracioso.usa> wrote:
>>> Stainless scratches if you touch it and then you make it look worse when you
>>> try to polish it.

>> It takes more than a touch to scratch it as it is pretty tuff and it
>> is not hard to polish out scratches if you do it right. You just need
>> the right method and compound.
>> -----------------
>> TheSnoMan.com

>
> I have heard of Kentrol. They are supposed to be good. Anybody know
> anything about Rugged Ridge stainless hinges?
>


There are some 'real' bad suppliers of 'stainless' out there. The worst
was 'stealhorse' which had to dump the name and farm out under new names
because no one would buy their products anymore. Their 'stainless' came
rusted right in the package, literally, as I have seen a few.

I don't know what names they are trying to sucker people under these
days unfortunately, maybe others do?

Kentrol is known for stainless that lasts.

If you plan on off roading, plan on your hinges getting scratched. They
are the last place a branch hooks up on as it slides past your hood.
Snoman doesn't off road so he has no experience with 'custom pin
striping' on his J10 snowplow. LOL!

I have never seen any coatings that would stay on stainless over time.
They all chip off. Not saying some newer stuff might not stick, but...

If I ever get more money than I know what to do with, after I put a new
frame in my CJ7 Laredo, I might go with stainless hinges to match my
chrome and stainless 'Laredo' package.

Mike
86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
88 Cherokee 235 BFG AT's
Canadian Off Road Trips Photos: Non members can still view!
Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
(More Off Road album links at bottom of the view page)

Mike Romain 04-10-2007 03:54 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
Tracie wrote:
> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>>
>> <a...@gracioso.usa> wrote:
>>> Stainless scratches if you touch it and then you make it look worse when you
>>> try to polish it.

>> It takes more than a touch to scratch it as it is pretty tuff and it
>> is not hard to polish out scratches if you do it right. You just need
>> the right method and compound.
>> -----------------
>> TheSnoMan.com

>
> I have heard of Kentrol. They are supposed to be good. Anybody know
> anything about Rugged Ridge stainless hinges?
>


There are some 'real' bad suppliers of 'stainless' out there. The worst
was 'stealhorse' which had to dump the name and farm out under new names
because no one would buy their products anymore. Their 'stainless' came
rusted right in the package, literally, as I have seen a few.

I don't know what names they are trying to sucker people under these
days unfortunately, maybe others do?

Kentrol is known for stainless that lasts.

If you plan on off roading, plan on your hinges getting scratched. They
are the last place a branch hooks up on as it slides past your hood.
Snoman doesn't off road so he has no experience with 'custom pin
striping' on his J10 snowplow. LOL!

I have never seen any coatings that would stay on stainless over time.
They all chip off. Not saying some newer stuff might not stick, but...

If I ever get more money than I know what to do with, after I put a new
frame in my CJ7 Laredo, I might go with stainless hinges to match my
chrome and stainless 'Laredo' package.

Mike
86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
88 Cherokee 235 BFG AT's
Canadian Off Road Trips Photos: Non members can still view!
Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
(More Off Road album links at bottom of the view page)

Mike Romain 04-10-2007 03:54 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
Tracie wrote:
> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>>
>> <a...@gracioso.usa> wrote:
>>> Stainless scratches if you touch it and then you make it look worse when you
>>> try to polish it.

>> It takes more than a touch to scratch it as it is pretty tuff and it
>> is not hard to polish out scratches if you do it right. You just need
>> the right method and compound.
>> -----------------
>> TheSnoMan.com

>
> I have heard of Kentrol. They are supposed to be good. Anybody know
> anything about Rugged Ridge stainless hinges?
>


There are some 'real' bad suppliers of 'stainless' out there. The worst
was 'stealhorse' which had to dump the name and farm out under new names
because no one would buy their products anymore. Their 'stainless' came
rusted right in the package, literally, as I have seen a few.

I don't know what names they are trying to sucker people under these
days unfortunately, maybe others do?

Kentrol is known for stainless that lasts.

If you plan on off roading, plan on your hinges getting scratched. They
are the last place a branch hooks up on as it slides past your hood.
Snoman doesn't off road so he has no experience with 'custom pin
striping' on his J10 snowplow. LOL!

I have never seen any coatings that would stay on stainless over time.
They all chip off. Not saying some newer stuff might not stick, but...

If I ever get more money than I know what to do with, after I put a new
frame in my CJ7 Laredo, I might go with stainless hinges to match my
chrome and stainless 'Laredo' package.

Mike
86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
88 Cherokee 235 BFG AT's
Canadian Off Road Trips Photos: Non members can still view!
Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
(More Off Road album links at bottom of the view page)

SnoMan 04-10-2007 06:08 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 15:54:52 -0400, Mike Romain <romainm@sympatico.ca>
wrote:

>Tracie wrote:
>> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
>>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>>>
>>> <a...@gracioso.usa> wrote:
>>>> Stainless scratches if you touch it and then you make it look worse when you
>>>> try to polish it.
>>> It takes more than a touch to scratch it as it is pretty tuff and it
>>> is not hard to polish out scratches if you do it right. You just need
>>> the right method and compound.
>>> -----------------
>>> TheSnoMan.com

>>
>> I have heard of Kentrol. They are supposed to be good. Anybody know
>> anything about Rugged Ridge stainless hinges?
>>

>
>There are some 'real' bad suppliers of 'stainless' out there. The worst
>was 'stealhorse' which had to dump the name and farm out under new names
>because no one would buy their products anymore. Their 'stainless' came
>rusted right in the package, literally, as I have seen a few.
>
>I don't know what names they are trying to sucker people under these
>days unfortunately, maybe others do?
>
>Kentrol is known for stainless that lasts.
>
>If you plan on off roading, plan on your hinges getting scratched. They
>are the last place a branch hooks up on as it slides past your hood.
>Snoman doesn't off road so he has no experience with 'custom pin
>striping' on his J10 snowplow. LOL!
>
>I have never seen any coatings that would stay on stainless over time.
>They all chip off. Not saying some newer stuff might not stick, but...
>
>If I ever get more money than I know what to do with, after I put a new
>frame in my CJ7 Laredo, I might go with stainless hinges to match my
>chrome and stainless 'Laredo' package.
>
>Mike
>86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
>88 Cherokee 235 BFG AT's
>Canadian Off Road Trips Photos: Non members can still view!
>Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
>(More Off Road album links at bottom of the view page)



The alloy SS it is play a big roll in quality too. I would ask them
what alloy they are using because some SS alloys are not good for
this. (they use them because it is easier to machine)
-----------------
TheSnoMan.com

SnoMan 04-10-2007 06:08 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 15:54:52 -0400, Mike Romain <romainm@sympatico.ca>
wrote:

>Tracie wrote:
>> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
>>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>>>
>>> <a...@gracioso.usa> wrote:
>>>> Stainless scratches if you touch it and then you make it look worse when you
>>>> try to polish it.
>>> It takes more than a touch to scratch it as it is pretty tuff and it
>>> is not hard to polish out scratches if you do it right. You just need
>>> the right method and compound.
>>> -----------------
>>> TheSnoMan.com

>>
>> I have heard of Kentrol. They are supposed to be good. Anybody know
>> anything about Rugged Ridge stainless hinges?
>>

>
>There are some 'real' bad suppliers of 'stainless' out there. The worst
>was 'stealhorse' which had to dump the name and farm out under new names
>because no one would buy their products anymore. Their 'stainless' came
>rusted right in the package, literally, as I have seen a few.
>
>I don't know what names they are trying to sucker people under these
>days unfortunately, maybe others do?
>
>Kentrol is known for stainless that lasts.
>
>If you plan on off roading, plan on your hinges getting scratched. They
>are the last place a branch hooks up on as it slides past your hood.
>Snoman doesn't off road so he has no experience with 'custom pin
>striping' on his J10 snowplow. LOL!
>
>I have never seen any coatings that would stay on stainless over time.
>They all chip off. Not saying some newer stuff might not stick, but...
>
>If I ever get more money than I know what to do with, after I put a new
>frame in my CJ7 Laredo, I might go with stainless hinges to match my
>chrome and stainless 'Laredo' package.
>
>Mike
>86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
>88 Cherokee 235 BFG AT's
>Canadian Off Road Trips Photos: Non members can still view!
>Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
>(More Off Road album links at bottom of the view page)



The alloy SS it is play a big roll in quality too. I would ask them
what alloy they are using because some SS alloys are not good for
this. (they use them because it is easier to machine)
-----------------
TheSnoMan.com

SnoMan 04-10-2007 06:08 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 15:54:52 -0400, Mike Romain <romainm@sympatico.ca>
wrote:

>Tracie wrote:
>> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
>>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
>>>
>>> <a...@gracioso.usa> wrote:
>>>> Stainless scratches if you touch it and then you make it look worse when you
>>>> try to polish it.
>>> It takes more than a touch to scratch it as it is pretty tuff and it
>>> is not hard to polish out scratches if you do it right. You just need
>>> the right method and compound.
>>> -----------------
>>> TheSnoMan.com

>>
>> I have heard of Kentrol. They are supposed to be good. Anybody know
>> anything about Rugged Ridge stainless hinges?
>>

>
>There are some 'real' bad suppliers of 'stainless' out there. The worst
>was 'stealhorse' which had to dump the name and farm out under new names
>because no one would buy their products anymore. Their 'stainless' came
>rusted right in the package, literally, as I have seen a few.
>
>I don't know what names they are trying to sucker people under these
>days unfortunately, maybe others do?
>
>Kentrol is known for stainless that lasts.
>
>If you plan on off roading, plan on your hinges getting scratched. They
>are the last place a branch hooks up on as it slides past your hood.
>Snoman doesn't off road so he has no experience with 'custom pin
>striping' on his J10 snowplow. LOL!
>
>I have never seen any coatings that would stay on stainless over time.
>They all chip off. Not saying some newer stuff might not stick, but...
>
>If I ever get more money than I know what to do with, after I put a new
>frame in my CJ7 Laredo, I might go with stainless hinges to match my
>chrome and stainless 'Laredo' package.
>
>Mike
>86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
>88 Cherokee 235 BFG AT's
>Canadian Off Road Trips Photos: Non members can still view!
>Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
>(More Off Road album links at bottom of the view page)



The alloy SS it is play a big roll in quality too. I would ask them
what alloy they are using because some SS alloys are not good for
this. (they use them because it is easier to machine)
-----------------
TheSnoMan.com

Earle Horton 04-10-2007 06:41 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
"SnoMan" <admin@snoman.com> wrote in message
news:kk2o135kqfkumnp78sd2lrm4bv8gnjf3pi@4ax.com...
> On Tue, 10 Apr 2007 15:54:52 -0400, Mike Romain <romainm@sympatico.ca>
> wrote:
>
> >Tracie wrote:
> >> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
> >>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
> >>>
> >>> <a...@gracioso.usa> wrote:
> >>>> Stainless scratches if you touch it and then you make it look worse

when you
> >>>> try to polish it.
> >>> It takes more than a touch to scratch it as it is pretty tuff and it
> >>> is not hard to polish out scratches if you do it right. You just need
> >>> the right method and compound.
> >>> -----------------
> >>> TheSnoMan.com
> >>
> >> I have heard of Kentrol. They are supposed to be good. Anybody know
> >> anything about Rugged Ridge stainless hinges?
> >>

> >
> >There are some 'real' bad suppliers of 'stainless' out there. The worst
> >was 'stealhorse' which had to dump the name and farm out under new names
> >because no one would buy their products anymore. Their 'stainless' came
> >rusted right in the package, literally, as I have seen a few.
> >
> >I don't know what names they are trying to sucker people under these
> >days unfortunately, maybe others do?
> >
> >Kentrol is known for stainless that lasts.
> >
> >If you plan on off roading, plan on your hinges getting scratched. They
> >are the last place a branch hooks up on as it slides past your hood.
> >Snoman doesn't off road so he has no experience with 'custom pin
> >striping' on his J10 snowplow. LOL!
> >
> >I have never seen any coatings that would stay on stainless over time.
> >They all chip off. Not saying some newer stuff might not stick, but...
> >
> >If I ever get more money than I know what to do with, after I put a new
> >frame in my CJ7 Laredo, I might go with stainless hinges to match my
> >chrome and stainless 'Laredo' package.
> >
> >Mike
> >86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
> >88 Cherokee 235 BFG AT's
> >Canadian Off Road Trips Photos: Non members can still view!
> >Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
> >(More Off Road album links at bottom of the view page)

>
>
> The alloy SS it is play a big roll in quality too. I would ask them
> what alloy they are using because some SS alloys are not good for
> this. (they use them because it is easier to machine)
> -----------------
> TheSnoMan.com


Heh, unless you're a metallurgist what they tell you will be meaningless.
There is of course a compromise between durability and machine-ability.
Watch out for "chrome" parts too. Chrome plating is a different process
than stainless. Are there lots of stainless and chromed J-10 parts
available?

Saludos,

Earle



Earle Horton 04-10-2007 06:41 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
"SnoMan" <admin@snoman.com> wrote in message
news:kk2o135kqfkumnp78sd2lrm4bv8gnjf3pi@4ax.com...
> On Tue, 10 Apr 2007 15:54:52 -0400, Mike Romain <romainm@sympatico.ca>
> wrote:
>
> >Tracie wrote:
> >> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
> >>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
> >>>
> >>> <a...@gracioso.usa> wrote:
> >>>> Stainless scratches if you touch it and then you make it look worse

when you
> >>>> try to polish it.
> >>> It takes more than a touch to scratch it as it is pretty tuff and it
> >>> is not hard to polish out scratches if you do it right. You just need
> >>> the right method and compound.
> >>> -----------------
> >>> TheSnoMan.com
> >>
> >> I have heard of Kentrol. They are supposed to be good. Anybody know
> >> anything about Rugged Ridge stainless hinges?
> >>

> >
> >There are some 'real' bad suppliers of 'stainless' out there. The worst
> >was 'stealhorse' which had to dump the name and farm out under new names
> >because no one would buy their products anymore. Their 'stainless' came
> >rusted right in the package, literally, as I have seen a few.
> >
> >I don't know what names they are trying to sucker people under these
> >days unfortunately, maybe others do?
> >
> >Kentrol is known for stainless that lasts.
> >
> >If you plan on off roading, plan on your hinges getting scratched. They
> >are the last place a branch hooks up on as it slides past your hood.
> >Snoman doesn't off road so he has no experience with 'custom pin
> >striping' on his J10 snowplow. LOL!
> >
> >I have never seen any coatings that would stay on stainless over time.
> >They all chip off. Not saying some newer stuff might not stick, but...
> >
> >If I ever get more money than I know what to do with, after I put a new
> >frame in my CJ7 Laredo, I might go with stainless hinges to match my
> >chrome and stainless 'Laredo' package.
> >
> >Mike
> >86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
> >88 Cherokee 235 BFG AT's
> >Canadian Off Road Trips Photos: Non members can still view!
> >Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
> >(More Off Road album links at bottom of the view page)

>
>
> The alloy SS it is play a big roll in quality too. I would ask them
> what alloy they are using because some SS alloys are not good for
> this. (they use them because it is easier to machine)
> -----------------
> TheSnoMan.com


Heh, unless you're a metallurgist what they tell you will be meaningless.
There is of course a compromise between durability and machine-ability.
Watch out for "chrome" parts too. Chrome plating is a different process
than stainless. Are there lots of stainless and chromed J-10 parts
available?

Saludos,

Earle



Earle Horton 04-10-2007 06:41 PM

Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
"SnoMan" <admin@snoman.com> wrote in message
news:kk2o135kqfkumnp78sd2lrm4bv8gnjf3pi@4ax.com...
> On Tue, 10 Apr 2007 15:54:52 -0400, Mike Romain <romainm@sympatico.ca>
> wrote:
>
> >Tracie wrote:
> >> On Apr 10, 2:40 pm, SnoMan <a...@snoman.com> wrote:
> >>> On Tue, 10 Apr 2007 12:03:59 -0600, "Earle Horton"
> >>>
> >>> <a...@gracioso.usa> wrote:
> >>>> Stainless scratches if you touch it and then you make it look worse

when you
> >>>> try to polish it.
> >>> It takes more than a touch to scratch it as it is pretty tuff and it
> >>> is not hard to polish out scratches if you do it right. You just need
> >>> the right method and compound.
> >>> -----------------
> >>> TheSnoMan.com
> >>
> >> I have heard of Kentrol. They are supposed to be good. Anybody know
> >> anything about Rugged Ridge stainless hinges?
> >>

> >
> >There are some 'real' bad suppliers of 'stainless' out there. The worst
> >was 'stealhorse' which had to dump the name and farm out under new names
> >because no one would buy their products anymore. Their 'stainless' came
> >rusted right in the package, literally, as I have seen a few.
> >
> >I don't know what names they are trying to sucker people under these
> >days unfortunately, maybe others do?
> >
> >Kentrol is known for stainless that lasts.
> >
> >If you plan on off roading, plan on your hinges getting scratched. They
> >are the last place a branch hooks up on as it slides past your hood.
> >Snoman doesn't off road so he has no experience with 'custom pin
> >striping' on his J10 snowplow. LOL!
> >
> >I have never seen any coatings that would stay on stainless over time.
> >They all chip off. Not saying some newer stuff might not stick, but...
> >
> >If I ever get more money than I know what to do with, after I put a new
> >frame in my CJ7 Laredo, I might go with stainless hinges to match my
> >chrome and stainless 'Laredo' package.
> >
> >Mike
> >86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
> >88 Cherokee 235 BFG AT's
> >Canadian Off Road Trips Photos: Non members can still view!
> >Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
> >(More Off Road album links at bottom of the view page)

>
>
> The alloy SS it is play a big roll in quality too. I would ask them
> what alloy they are using because some SS alloys are not good for
> this. (they use them because it is easier to machine)
> -----------------
> TheSnoMan.com


Heh, unless you're a metallurgist what they tell you will be meaningless.
There is of course a compromise between durability and machine-ability.
Watch out for "chrome" parts too. Chrome plating is a different process
than stainless. Are there lots of stainless and chromed J-10 parts
available?

Saludos,

Earle



Heatwave 04-10-2007 08:25 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
romainm@sympatico.ca says...
> There are some 'real' bad suppliers of 'stainless' out there. The worst
> was 'stealhorse' which had to dump the name and farm out under new names
> because no one would buy their products anymore. Their 'stainless' came
> rusted right in the package, literally, as I have seen a few.


You want to look for 304 stainless. Most other grades have to much
carbon.

> I don't know what names they are trying to sucker people under these
> days unfortunately, maybe others do?
>
> Kentrol is known for stainless that lasts.
>
> If you plan on off roading, plan on your hinges getting scratched. They
> are the last place a branch hooks up on as it slides past your hood.
> Snoman doesn't off road so he has no experience with 'custom pin
> striping' on his J10 snowplow. LOL!
>
> I have never seen any coatings that would stay on stainless over time.
> They all chip off. Not saying some newer stuff might not stick, but...


Don't bother painting stainless... IMO it seems pointless even if you do
get it to stick.

> If I ever get more money than I know what to do with, after I put a new
> frame in my CJ7 Laredo, I might go with stainless hinges to match my
> chrome and stainless 'Laredo' package.
>
> Mike
> 86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
> 88 Cherokee 235 BFG AT's
> Canadian Off Road Trips Photos: Non members can still view!
> Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
> (More Off Road album links at bottom of the view page)



Heatwave 04-10-2007 08:25 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
romainm@sympatico.ca says...
> There are some 'real' bad suppliers of 'stainless' out there. The worst
> was 'stealhorse' which had to dump the name and farm out under new names
> because no one would buy their products anymore. Their 'stainless' came
> rusted right in the package, literally, as I have seen a few.


You want to look for 304 stainless. Most other grades have to much
carbon.

> I don't know what names they are trying to sucker people under these
> days unfortunately, maybe others do?
>
> Kentrol is known for stainless that lasts.
>
> If you plan on off roading, plan on your hinges getting scratched. They
> are the last place a branch hooks up on as it slides past your hood.
> Snoman doesn't off road so he has no experience with 'custom pin
> striping' on his J10 snowplow. LOL!
>
> I have never seen any coatings that would stay on stainless over time.
> They all chip off. Not saying some newer stuff might not stick, but...


Don't bother painting stainless... IMO it seems pointless even if you do
get it to stick.

> If I ever get more money than I know what to do with, after I put a new
> frame in my CJ7 Laredo, I might go with stainless hinges to match my
> chrome and stainless 'Laredo' package.
>
> Mike
> 86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
> 88 Cherokee 235 BFG AT's
> Canadian Off Road Trips Photos: Non members can still view!
> Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
> (More Off Road album links at bottom of the view page)



Heatwave 04-10-2007 08:25 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
romainm@sympatico.ca says...
> There are some 'real' bad suppliers of 'stainless' out there. The worst
> was 'stealhorse' which had to dump the name and farm out under new names
> because no one would buy their products anymore. Their 'stainless' came
> rusted right in the package, literally, as I have seen a few.


You want to look for 304 stainless. Most other grades have to much
carbon.

> I don't know what names they are trying to sucker people under these
> days unfortunately, maybe others do?
>
> Kentrol is known for stainless that lasts.
>
> If you plan on off roading, plan on your hinges getting scratched. They
> are the last place a branch hooks up on as it slides past your hood.
> Snoman doesn't off road so he has no experience with 'custom pin
> striping' on his J10 snowplow. LOL!
>
> I have never seen any coatings that would stay on stainless over time.
> They all chip off. Not saying some newer stuff might not stick, but...


Don't bother painting stainless... IMO it seems pointless even if you do
get it to stick.

> If I ever get more money than I know what to do with, after I put a new
> frame in my CJ7 Laredo, I might go with stainless hinges to match my
> chrome and stainless 'Laredo' package.
>
> Mike
> 86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
> 88 Cherokee 235 BFG AT's
> Canadian Off Road Trips Photos: Non members can still view!
> Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
> (More Off Road album links at bottom of the view page)



reboot 04-10-2007 09:15 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
<m3lt1ng5n0wmen@wah00.com> wrote:

>In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>romainm@sympatico.ca says...
>> There are some 'real' bad suppliers of 'stainless' out there. The worst
>> was 'stealhorse' which had to dump the name and farm out under new names
>> because no one would buy their products anymore. Their 'stainless' came
>> rusted right in the package, literally, as I have seen a few.

>
>You want to look for 304 stainless. Most other grades have to much
>carbon.
>
>> I don't know what names they are trying to sucker people under these
>> days unfortunately, maybe others do?
>>
>> Kentrol is known for stainless that lasts.
>>
>> If you plan on off roading, plan on your hinges getting scratched. They
>> are the last place a branch hooks up on as it slides past your hood.
>> Snoman doesn't off road so he has no experience with 'custom pin
>> striping' on his J10 snowplow. LOL!
>>
>> I have never seen any coatings that would stay on stainless over time.
>> They all chip off. Not saying some newer stuff might not stick, but...

>
>Don't bother painting stainless... IMO it seems pointless even if you do
>get it to stick.
>
>> If I ever get more money than I know what to do with, after I put a new
>> frame in my CJ7 Laredo, I might go with stainless hinges to match my
>> chrome and stainless 'Laredo' package.
>>
>> Mike
>> 86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
>> 88 Cherokee 235 BFG AT's
>> Canadian Off Road Trips Photos: Non members can still view!
>> Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
>> (More Off Road album links at bottom of the view page)


hi all,
304 SS is also known as muffler stainless, it isn't a high grade of
stainless steel, it is pretty soft (as SS goes), it is easily machined
(especially with an L alloyed in) or formed / bent. corrosion
resistance (penetration resistance) is pretty good but for cosmetic
applications it won't hold a high polish or resist scratches.

most u.s. built cars / trucks with SS exhaust systems use 304 SS.

it will not however red rust or white corrode which would already be a
big improvement over the hinges and mirror brackets on my TJ.

reboot


---
avast! Antivirus: Outbound message clean.
Virus Database (VPS): 000732-0, 04/10/2007
Tested on: 4/10/2007 9:15:25 PM
avast! - copyright (c) 1988-2007 ALWIL Software.
http://www.avast.com




reboot 04-10-2007 09:15 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
<m3lt1ng5n0wmen@wah00.com> wrote:

>In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>romainm@sympatico.ca says...
>> There are some 'real' bad suppliers of 'stainless' out there. The worst
>> was 'stealhorse' which had to dump the name and farm out under new names
>> because no one would buy their products anymore. Their 'stainless' came
>> rusted right in the package, literally, as I have seen a few.

>
>You want to look for 304 stainless. Most other grades have to much
>carbon.
>
>> I don't know what names they are trying to sucker people under these
>> days unfortunately, maybe others do?
>>
>> Kentrol is known for stainless that lasts.
>>
>> If you plan on off roading, plan on your hinges getting scratched. They
>> are the last place a branch hooks up on as it slides past your hood.
>> Snoman doesn't off road so he has no experience with 'custom pin
>> striping' on his J10 snowplow. LOL!
>>
>> I have never seen any coatings that would stay on stainless over time.
>> They all chip off. Not saying some newer stuff might not stick, but...

>
>Don't bother painting stainless... IMO it seems pointless even if you do
>get it to stick.
>
>> If I ever get more money than I know what to do with, after I put a new
>> frame in my CJ7 Laredo, I might go with stainless hinges to match my
>> chrome and stainless 'Laredo' package.
>>
>> Mike
>> 86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
>> 88 Cherokee 235 BFG AT's
>> Canadian Off Road Trips Photos: Non members can still view!
>> Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
>> (More Off Road album links at bottom of the view page)


hi all,
304 SS is also known as muffler stainless, it isn't a high grade of
stainless steel, it is pretty soft (as SS goes), it is easily machined
(especially with an L alloyed in) or formed / bent. corrosion
resistance (penetration resistance) is pretty good but for cosmetic
applications it won't hold a high polish or resist scratches.

most u.s. built cars / trucks with SS exhaust systems use 304 SS.

it will not however red rust or white corrode which would already be a
big improvement over the hinges and mirror brackets on my TJ.

reboot


---
avast! Antivirus: Outbound message clean.
Virus Database (VPS): 000732-0, 04/10/2007
Tested on: 4/10/2007 9:15:25 PM
avast! - copyright (c) 1988-2007 ALWIL Software.
http://www.avast.com




reboot 04-10-2007 09:15 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
<m3lt1ng5n0wmen@wah00.com> wrote:

>In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>romainm@sympatico.ca says...
>> There are some 'real' bad suppliers of 'stainless' out there. The worst
>> was 'stealhorse' which had to dump the name and farm out under new names
>> because no one would buy their products anymore. Their 'stainless' came
>> rusted right in the package, literally, as I have seen a few.

>
>You want to look for 304 stainless. Most other grades have to much
>carbon.
>
>> I don't know what names they are trying to sucker people under these
>> days unfortunately, maybe others do?
>>
>> Kentrol is known for stainless that lasts.
>>
>> If you plan on off roading, plan on your hinges getting scratched. They
>> are the last place a branch hooks up on as it slides past your hood.
>> Snoman doesn't off road so he has no experience with 'custom pin
>> striping' on his J10 snowplow. LOL!
>>
>> I have never seen any coatings that would stay on stainless over time.
>> They all chip off. Not saying some newer stuff might not stick, but...

>
>Don't bother painting stainless... IMO it seems pointless even if you do
>get it to stick.
>
>> If I ever get more money than I know what to do with, after I put a new
>> frame in my CJ7 Laredo, I might go with stainless hinges to match my
>> chrome and stainless 'Laredo' package.
>>
>> Mike
>> 86/00 CJ7 Laredo, 33x9.5 BFG Muds, 'glass nose to tail in '00
>> 88 Cherokee 235 BFG AT's
>> Canadian Off Road Trips Photos: Non members can still view!
>> Jan/06 http://www.imagestation.com/album/pi...?id=2115147590
>> (More Off Road album links at bottom of the view page)


hi all,
304 SS is also known as muffler stainless, it isn't a high grade of
stainless steel, it is pretty soft (as SS goes), it is easily machined
(especially with an L alloyed in) or formed / bent. corrosion
resistance (penetration resistance) is pretty good but for cosmetic
applications it won't hold a high polish or resist scratches.

most u.s. built cars / trucks with SS exhaust systems use 304 SS.

it will not however red rust or white corrode which would already be a
big improvement over the hinges and mirror brackets on my TJ.

reboot


---
avast! Antivirus: Outbound message clean.
Virus Database (VPS): 000732-0, 04/10/2007
Tested on: 4/10/2007 9:15:25 PM
avast! - copyright (c) 1988-2007 ALWIL Software.
http://www.avast.com




SnoMan 04-10-2007 09:25 PM

Re: Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 16:41:11 -0600, "Earle Horton"
<apodo@gracioso.usa> wrote:

>Heh, unless you're a metallurgist what they tell you will be meaningless.



Not if you know how to look alloys up because you can find out in a
few minute or less on internt for ANY alloy or any metal. I used to
know the major alloys but I would have to look them up to. (I still
remember some steel and aluminum ones though)
-----------------
TheSnoMan.com

SnoMan 04-10-2007 09:25 PM

Re: Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 16:41:11 -0600, "Earle Horton"
<apodo@gracioso.usa> wrote:

>Heh, unless you're a metallurgist what they tell you will be meaningless.



Not if you know how to look alloys up because you can find out in a
few minute or less on internt for ANY alloy or any metal. I used to
know the major alloys but I would have to look them up to. (I still
remember some steel and aluminum ones though)
-----------------
TheSnoMan.com

SnoMan 04-10-2007 09:25 PM

Re: Re: Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Tue, 10 Apr 2007 16:41:11 -0600, "Earle Horton"
<apodo@gracioso.usa> wrote:

>Heh, unless you're a metallurgist what they tell you will be meaningless.



Not if you know how to look alloys up because you can find out in a
few minute or less on internt for ANY alloy or any metal. I used to
know the major alloys but I would have to look them up to. (I still
remember some steel and aluminum ones though)
-----------------
TheSnoMan.com

Heatwave 04-10-2007 10:54 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
reboot@nothere.newsguy.com says...
> On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
> <m3lt1ng5n0wmen@wah00.com> wrote:


> >In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
> >romainm@sympatico.ca says...
> >>
> >> Kentrol is known for stainless that lasts.
> >>

[snips]

> hi all,
> 304 SS is also known as muffler stainless, it isn't a high grade of
> stainless steel, it is pretty soft (as SS goes), it is easily machined
> (especially with an L alloyed in) or formed / bent. corrosion
> resistance (penetration resistance) is pretty good but for cosmetic
> applications it won't hold a high polish or resist scratches.
>
> most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>
> it will not however red rust or white corrode which would already be a
> big improvement over the hinges and mirror brackets on my TJ.
>
> reboot


I use 304 for my chopper parts and they seem to hold a polish. I googled
Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I just
thought I'd say if you are looking for stainless parts and they don't
state "304" stainless you might want to stay clear of them so you don't
run into the same problem Mike did. 316 is another good alloy of
stainless...if you ever see parts made from it.

Heatwave 04-10-2007 10:54 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
reboot@nothere.newsguy.com says...
> On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
> <m3lt1ng5n0wmen@wah00.com> wrote:


> >In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
> >romainm@sympatico.ca says...
> >>
> >> Kentrol is known for stainless that lasts.
> >>

[snips]

> hi all,
> 304 SS is also known as muffler stainless, it isn't a high grade of
> stainless steel, it is pretty soft (as SS goes), it is easily machined
> (especially with an L alloyed in) or formed / bent. corrosion
> resistance (penetration resistance) is pretty good but for cosmetic
> applications it won't hold a high polish or resist scratches.
>
> most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>
> it will not however red rust or white corrode which would already be a
> big improvement over the hinges and mirror brackets on my TJ.
>
> reboot


I use 304 for my chopper parts and they seem to hold a polish. I googled
Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I just
thought I'd say if you are looking for stainless parts and they don't
state "304" stainless you might want to stay clear of them so you don't
run into the same problem Mike did. 316 is another good alloy of
stainless...if you ever see parts made from it.

Heatwave 04-10-2007 10:54 PM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
reboot@nothere.newsguy.com says...
> On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
> <m3lt1ng5n0wmen@wah00.com> wrote:


> >In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
> >romainm@sympatico.ca says...
> >>
> >> Kentrol is known for stainless that lasts.
> >>

[snips]

> hi all,
> 304 SS is also known as muffler stainless, it isn't a high grade of
> stainless steel, it is pretty soft (as SS goes), it is easily machined
> (especially with an L alloyed in) or formed / bent. corrosion
> resistance (penetration resistance) is pretty good but for cosmetic
> applications it won't hold a high polish or resist scratches.
>
> most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>
> it will not however red rust or white corrode which would already be a
> big improvement over the hinges and mirror brackets on my TJ.
>
> reboot


I use 304 for my chopper parts and they seem to hold a polish. I googled
Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I just
thought I'd say if you are looking for stainless parts and they don't
state "304" stainless you might want to stay clear of them so you don't
run into the same problem Mike did. 316 is another good alloy of
stainless...if you ever see parts made from it.

c 04-11-2007 08:17 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
316 Stainless is the alloy most used on the parts we make for the local
shipyard here, obviously for corrosion resistance. The corrosion
resistance is superior to most other stainless alloys, but expect to pay
for it. Not only is the metal more expensive, it is a bitch to machine
compared to 303 or 304. This stuff will wear out carbide tooling in our
CNC lathe easily 5 times faster than 303/304 will.

Chris

FrankW wrote:
> When I was into salt water aquariums I was looking
> up Stainless steel for use with them.
> If I remember correctly
> 304 stainless will last 10 years before it "starts" to corrode.
> 316 stainless will last 100 years before it starts to corrode
> submersed in saltwater.
>
> Heatwave wrote:
>> In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
>> reboot@nothere.newsguy.com says...
>>
>>> On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
>>> <m3lt1ng5n0wmen@wah00.com> wrote:

>>
>>
>>>> In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>>>> romainm@sympatico.ca says...
>>>>
>>>>> Kentrol is known for stainless that lasts.
>>>>>

>>
>> [snips]
>>
>>
>>> hi all,
>>> 304 SS is also known as muffler stainless, it isn't a high grade of
>>> stainless steel, it is pretty soft (as SS goes), it is easily machined
>>> (especially with an L alloyed in) or formed / bent. corrosion
>>> resistance (penetration resistance) is pretty good but for cosmetic
>>> applications it won't hold a high polish or resist scratches.
>>>
>>> most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>>>
>>> it will not however red rust or white corrode which would already be a
>>> big improvement over the hinges and mirror brackets on my TJ.
>>>
>>> reboot

>>
>>
>> I use 304 for my chopper parts and they seem to hold a polish. I
>> googled Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I
>> just thought I'd say if you are looking for stainless parts and they
>> don't state "304" stainless you might want to stay clear of them so
>> you don't run into the same problem Mike did. 316 is another good
>> alloy of stainless...if you ever see parts made from it.

>


c 04-11-2007 08:17 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
316 Stainless is the alloy most used on the parts we make for the local
shipyard here, obviously for corrosion resistance. The corrosion
resistance is superior to most other stainless alloys, but expect to pay
for it. Not only is the metal more expensive, it is a bitch to machine
compared to 303 or 304. This stuff will wear out carbide tooling in our
CNC lathe easily 5 times faster than 303/304 will.

Chris

FrankW wrote:
> When I was into salt water aquariums I was looking
> up Stainless steel for use with them.
> If I remember correctly
> 304 stainless will last 10 years before it "starts" to corrode.
> 316 stainless will last 100 years before it starts to corrode
> submersed in saltwater.
>
> Heatwave wrote:
>> In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
>> reboot@nothere.newsguy.com says...
>>
>>> On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
>>> <m3lt1ng5n0wmen@wah00.com> wrote:

>>
>>
>>>> In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>>>> romainm@sympatico.ca says...
>>>>
>>>>> Kentrol is known for stainless that lasts.
>>>>>

>>
>> [snips]
>>
>>
>>> hi all,
>>> 304 SS is also known as muffler stainless, it isn't a high grade of
>>> stainless steel, it is pretty soft (as SS goes), it is easily machined
>>> (especially with an L alloyed in) or formed / bent. corrosion
>>> resistance (penetration resistance) is pretty good but for cosmetic
>>> applications it won't hold a high polish or resist scratches.
>>>
>>> most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>>>
>>> it will not however red rust or white corrode which would already be a
>>> big improvement over the hinges and mirror brackets on my TJ.
>>>
>>> reboot

>>
>>
>> I use 304 for my chopper parts and they seem to hold a polish. I
>> googled Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I
>> just thought I'd say if you are looking for stainless parts and they
>> don't state "304" stainless you might want to stay clear of them so
>> you don't run into the same problem Mike did. 316 is another good
>> alloy of stainless...if you ever see parts made from it.

>


c 04-11-2007 08:17 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
316 Stainless is the alloy most used on the parts we make for the local
shipyard here, obviously for corrosion resistance. The corrosion
resistance is superior to most other stainless alloys, but expect to pay
for it. Not only is the metal more expensive, it is a bitch to machine
compared to 303 or 304. This stuff will wear out carbide tooling in our
CNC lathe easily 5 times faster than 303/304 will.

Chris

FrankW wrote:
> When I was into salt water aquariums I was looking
> up Stainless steel for use with them.
> If I remember correctly
> 304 stainless will last 10 years before it "starts" to corrode.
> 316 stainless will last 100 years before it starts to corrode
> submersed in saltwater.
>
> Heatwave wrote:
>> In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
>> reboot@nothere.newsguy.com says...
>>
>>> On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
>>> <m3lt1ng5n0wmen@wah00.com> wrote:

>>
>>
>>>> In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>>>> romainm@sympatico.ca says...
>>>>
>>>>> Kentrol is known for stainless that lasts.
>>>>>

>>
>> [snips]
>>
>>
>>> hi all,
>>> 304 SS is also known as muffler stainless, it isn't a high grade of
>>> stainless steel, it is pretty soft (as SS goes), it is easily machined
>>> (especially with an L alloyed in) or formed / bent. corrosion
>>> resistance (penetration resistance) is pretty good but for cosmetic
>>> applications it won't hold a high polish or resist scratches.
>>>
>>> most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>>>
>>> it will not however red rust or white corrode which would already be a
>>> big improvement over the hinges and mirror brackets on my TJ.
>>>
>>> reboot

>>
>>
>> I use 304 for my chopper parts and they seem to hold a polish. I
>> googled Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I
>> just thought I'd say if you are looking for stainless parts and they
>> don't state "304" stainless you might want to stay clear of them so
>> you don't run into the same problem Mike did. 316 is another good
>> alloy of stainless...if you ever see parts made from it.

>


FrankW 04-11-2007 08:49 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
When I was into salt water aquariums I was looking
up Stainless steel for use with them.
If I remember correctly
304 stainless will last 10 years before it "starts" to corrode.
316 stainless will last 100 years before it starts to corrode
submersed in saltwater.

Heatwave wrote:
> In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
> reboot@nothere.newsguy.com says...
>
>>On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
>><m3lt1ng5n0wmen@wah00.com> wrote:

>
>
>>>In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>>>romainm@sympatico.ca says...
>>>
>>>>Kentrol is known for stainless that lasts.
>>>>

>
> [snips]
>
>
>>hi all,
>>304 SS is also known as muffler stainless, it isn't a high grade of
>>stainless steel, it is pretty soft (as SS goes), it is easily machined
>>(especially with an L alloyed in) or formed / bent. corrosion
>>resistance (penetration resistance) is pretty good but for cosmetic
>>applications it won't hold a high polish or resist scratches.
>>
>>most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>>
>>it will not however red rust or white corrode which would already be a
>>big improvement over the hinges and mirror brackets on my TJ.
>>
>>reboot

>
>
> I use 304 for my chopper parts and they seem to hold a polish. I googled
> Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I just
> thought I'd say if you are looking for stainless parts and they don't
> state "304" stainless you might want to stay clear of them so you don't
> run into the same problem Mike did. 316 is another good alloy of
> stainless...if you ever see parts made from it.



FrankW 04-11-2007 08:49 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
When I was into salt water aquariums I was looking
up Stainless steel for use with them.
If I remember correctly
304 stainless will last 10 years before it "starts" to corrode.
316 stainless will last 100 years before it starts to corrode
submersed in saltwater.

Heatwave wrote:
> In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
> reboot@nothere.newsguy.com says...
>
>>On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
>><m3lt1ng5n0wmen@wah00.com> wrote:

>
>
>>>In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>>>romainm@sympatico.ca says...
>>>
>>>>Kentrol is known for stainless that lasts.
>>>>

>
> [snips]
>
>
>>hi all,
>>304 SS is also known as muffler stainless, it isn't a high grade of
>>stainless steel, it is pretty soft (as SS goes), it is easily machined
>>(especially with an L alloyed in) or formed / bent. corrosion
>>resistance (penetration resistance) is pretty good but for cosmetic
>>applications it won't hold a high polish or resist scratches.
>>
>>most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>>
>>it will not however red rust or white corrode which would already be a
>>big improvement over the hinges and mirror brackets on my TJ.
>>
>>reboot

>
>
> I use 304 for my chopper parts and they seem to hold a polish. I googled
> Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I just
> thought I'd say if you are looking for stainless parts and they don't
> state "304" stainless you might want to stay clear of them so you don't
> run into the same problem Mike did. 316 is another good alloy of
> stainless...if you ever see parts made from it.



FrankW 04-11-2007 08:49 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
When I was into salt water aquariums I was looking
up Stainless steel for use with them.
If I remember correctly
304 stainless will last 10 years before it "starts" to corrode.
316 stainless will last 100 years before it starts to corrode
submersed in saltwater.

Heatwave wrote:
> In article <ubdo135bplo1e2a5ho5ojkfhuh5pug5nvo@4ax.com>,
> reboot@nothere.newsguy.com says...
>
>>On Tue, 10 Apr 2007 20:25:09 -0400, Heatwave
>><m3lt1ng5n0wmen@wah00.com> wrote:

>
>
>>>In article <461beb7a$0$22696$9a6e19ea@unlimited.newshosting.c om>,
>>>romainm@sympatico.ca says...
>>>
>>>>Kentrol is known for stainless that lasts.
>>>>

>
> [snips]
>
>
>>hi all,
>>304 SS is also known as muffler stainless, it isn't a high grade of
>>stainless steel, it is pretty soft (as SS goes), it is easily machined
>>(especially with an L alloyed in) or formed / bent. corrosion
>>resistance (penetration resistance) is pretty good but for cosmetic
>>applications it won't hold a high polish or resist scratches.
>>
>>most u.s. built cars / trucks with SS exhaust systems use 304 SS.
>>
>>it will not however red rust or white corrode which would already be a
>>big improvement over the hinges and mirror brackets on my TJ.
>>
>>reboot

>
>
> I use 304 for my chopper parts and they seem to hold a polish. I googled
> Kentrol + 304 and found Kentrol uses a lot of 304 stainless. I just
> thought I'd say if you are looking for stainless parts and they don't
> state "304" stainless you might want to stay clear of them so you don't
> run into the same problem Mike did. 316 is another good alloy of
> stainless...if you ever see parts made from it.



SkyKing49 04-11-2007 10:28 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Apr 10, 1:32 pm, "Tracie" <brain...@upstate.edu> wrote:
> I am going to be replacing the windshield hinges, upper and lower door
> hinges, and hood hinges on my 2006WranglerX (just to prevent rust in
> the future). I am torn between getting the 304 stainless steel with
> the high polished mirror finish or the black chrome finish over the
> 304 stainless steel. My jeep is the Midnight Blue metallic (navy
> blue) color. Which one would look better? I also am going to be
> putting on nerf bars (preferably stainless) and would also like to
> install the euro guard headlight/side marker/parking/tail light guards
> but I am not sure which color of these yet (depends on the color of
> all the hinges). Anyone have any suggestions or know anything about
> the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
> would be greatly appreciated. THANKS



I own the same vehicle. Go all out and buy a grille cover and vent
cover. I also bought a new front bumper with the plastic inserts for
the ends..new tire cover..new bikini top and deck cover. Oh yes..and
new tow hooks. I am not going to be doing any serious off-roading
until my Jeep gets old but to do trail rides in Ct. you must have tow
hooks. Oh...and some Back Off mud guards.


SkyKing49 04-11-2007 10:28 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Apr 10, 1:32 pm, "Tracie" <brain...@upstate.edu> wrote:
> I am going to be replacing the windshield hinges, upper and lower door
> hinges, and hood hinges on my 2006WranglerX (just to prevent rust in
> the future). I am torn between getting the 304 stainless steel with
> the high polished mirror finish or the black chrome finish over the
> 304 stainless steel. My jeep is the Midnight Blue metallic (navy
> blue) color. Which one would look better? I also am going to be
> putting on nerf bars (preferably stainless) and would also like to
> install the euro guard headlight/side marker/parking/tail light guards
> but I am not sure which color of these yet (depends on the color of
> all the hinges). Anyone have any suggestions or know anything about
> the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
> would be greatly appreciated. THANKS



I own the same vehicle. Go all out and buy a grille cover and vent
cover. I also bought a new front bumper with the plastic inserts for
the ends..new tire cover..new bikini top and deck cover. Oh yes..and
new tow hooks. I am not going to be doing any serious off-roading
until my Jeep gets old but to do trail rides in Ct. you must have tow
hooks. Oh...and some Back Off mud guards.


SkyKing49 04-11-2007 10:28 AM

Re: SILLY QUESTION -- JUST NEED AN OPINION FROM EVERYONE
 
On Apr 10, 1:32 pm, "Tracie" <brain...@upstate.edu> wrote:
> I am going to be replacing the windshield hinges, upper and lower door
> hinges, and hood hinges on my 2006WranglerX (just to prevent rust in
> the future). I am torn between getting the 304 stainless steel with
> the high polished mirror finish or the black chrome finish over the
> 304 stainless steel. My jeep is the Midnight Blue metallic (navy
> blue) color. Which one would look better? I also am going to be
> putting on nerf bars (preferably stainless) and would also like to
> install the euro guard headlight/side marker/parking/tail light guards
> but I am not sure which color of these yet (depends on the color of
> all the hinges). Anyone have any suggestions or know anything about
> the black chrome (i.e. does it flake, chip, peel, etc.)? Any comments
> would be greatly appreciated. THANKS



I own the same vehicle. Go all out and buy a grille cover and vent
cover. I also bought a new front bumper with the plastic inserts for
the ends..new tire cover..new bikini top and deck cover. Oh yes..and
new tow hooks. I am not going to be doing any serious off-roading
until my Jeep gets old but to do trail rides in Ct. you must have tow
hooks. Oh...and some Back Off mud guards.



All times are GMT -4. The time now is 06:29 AM.


© 2024 MH Sub I, LLC dba Internet Brands

Page generated in 0.06900 seconds with 4 queries